8–11 Jun 2026
SwissTech Convention Center EPFL
Europe/Zurich timezone

Session

Hydration 2

9 Jun 2026, 13:30
SwissTech Convention Center EPFL

SwissTech Convention Center EPFL

SwissTech Convention Center, EPFL, Rue Louis Favre 2, Ecublens, Switzerland

Conveners

Hydration 2

  • Barbara Lothenbach
  • Elsa Qoku

Presentation materials

There are no materials yet.

  1. Dr Julian Goergens
    09/06/2026, 13:30
    Hydration
    Oral Presentation

    Quantification of the metastable hydrate phases CAH10 and C2AHx is essential in understanding and evaluating the conversion progress of CAC pastes for scientific and industrial research. Mainly XRD or TGA are used for phase quantification, whereas XRD proved to be more precise. While structural data exist for CAH10, they do not yet exist for C2AHx, as the proportion of interlayer H2O in the...

    Go to contribution page
  2. Dr Andreas Koehler (Almatis GmbH)
    09/06/2026, 13:50
    Hydration
    Oral Presentation

    Calcium aluminate cement is widely used as a binder in refractory castables because it enables shaping complex geometries and allows the material to withstand extreme temperatures. Their typical manufacturing process consists of mixing, curing, demolding, drying and firing. In modern dense and highly dispersed castables with very low permeability, water remains in the castable body during the...

    Go to contribution page
  3. Jean Michel Auvray (IMERYS)
    09/06/2026, 14:10
    Hydration
    Oral Presentation

    High performance (HP) refractory concrete rely mainly on sophisticated, highly densified matrix systems with a high charge of pore-filling alumina and silica micro-powders, deflocculated with efficient polymer admixtures, and bonded with 70% Al2O3 containing calcium aluminate. However, these HP concretes experience a challenge concerning the safe and rapid removal of free pore and hydrate...

    Go to contribution page